MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials ARMATEX® SF45 Silicone Rubber Coated Glass Fabric
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: Description: Armatex Coatings are applied to base textiles that range in chemical composition, configuration and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based. The Polymer coatings include Silicone, Polyurethane, Acrylic, Teflon, Fluoroelastomer and hybrids. The Mineral coatings include Graphite, Quartz and hybrids. Textile fabric can be coated with a different coating on each side. The coatings are applied to most any Hytex cloth to enhance the performance characteristics of the base fabric in abrasion, chemical and heat resistance.

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 62.5 lb/ft³Calculated from weight of 45 oz/sy
Thickness 60.0 milGauge, nominal
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °FTreatment Limit, Continuous
 1000 °FFabric Limit, Continuous
 
Descriptive Properties
CoatingSilicone Rubber
ColorVarious
Flame Support ResistanceExcellent
Resistance to HydrocarbonsGood
Resistance to OilGood
Sides2
Standard Width40 or 60 inches
Water Penetration ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
CHT Group QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material
Mid-Mountain Materials ARMATEX® SRS 40 Silica Fabric Impregnated with Silicone Rubber
Mid-Mountain Materials ARMATEX® SF32 Silicone Rubber Coated Glass Fabric
Mid-Mountain Materials ARMATEX® SF37 Silicone Rubber Coated Glass Fabric

CMID27 / 1531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.