MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synthos WELLITE™ FR-90 Phenolic Resin for Friction Material
Categories: Polymer; Thermoset; Phenolic

Material Notes: This series of phenolic resin, FR-50/FR-90/FR-70N, is applied into the brake lining/pad/shoes, clutch disc and all kinds of friction materials for motorcycles, farm vehicle, cars, heavy truck and train brake shoe etc. It is characterized in good friction performance, wide adjusting range of friction ratios and good recovery ability in high temperature.

Application: Compared with F-50, it has higher purity and bonding strength and the product made of it has lower friction loss and more stable friction coefficient.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time 90.0 - 120 sec
@Temperature 150 °C
 
Descriptive Properties
AppearanceLight yellow powder
Content<1.5%Free phenol
Granularity99% under200 mesh
Inclined plate flow40-60 mm125°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW079 / 320110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.