MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® RLX-020 Polypropylene Extrusion/Blow-Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Random copolymer, antistatic for extrusion-blow molding

Note: 2002 - This product is no longer a part of the manufacturers product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.903 g/ccCompression-Molded; ASTM D1505
Melt Flow 1.8 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72Injection-Molded; ASTM D2240
Tensile Strength, Yield 31.0 MPaInjection-Molded; ASTM D638
Flexural Modulus 1.276 GPaTangent, 1.27 cm/min; ASTM D790; Compression-Molded
Izod Impact, Notched 0.370 J/cmASTM D256; Injection-Molded
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CInjection-Molded; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 °CFeed
 210 °CDie

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem RP 270G Extrusion Blow Molding Polypropylene
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
Dow DMDA-8907 NT 7 High Density Polyethylene Resin

PPPP0M / 57704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.