MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MIRATAINE® H2C-HA Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Biodegradable Sodium Laurimino Dipropionate (30%). Moderate foaming amphoteric surfactant, Excellent for cleaning hard surfaces. Stable in acidic and alkaline formulations. Very good hydrotrope. Compliant with the EU's detergent biodegradability regulation

Chemical Name: SODIUM LAURIMINO DIPROPIONATE

CAS: 14960-06-6

Compatibility: Compatible with anionic, cationic, and nonionic surfactants. Hard water compatible.

Character: Amphoteric

Stability: Excellent acid and alkaline stability.

Available in: Europe, Latin America and North America

Applications: MIRATAINE ® H-30 is a high foaming betaine surfactant that demonstrates excellent stability properties over broad pH ranges. Typically used as a secondary surfactant in anionic based systems, MIRATAINE ® H-30 improves overall foam quality and also helps improve formulation mildness.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 28 - 31 %Microwave; RP-0531
pH 6.0 - 7.0RP-0420
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 42 - 55RP-0007
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 69 - 72 %
 
Descriptive Properties
CompositionTotal Active28-31%, Solids

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® PA32 Surfactant
Solvay RHODAQUAT® M-242B/99 Surfactant
Solvay RHODAFAC® RE-610 Surfactant
Solvay MIRANOL® C2M-SF CONC Surfactant
Solvay GEROPON® HW 15 Surfactant

WRHOD289 / 137520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.