MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 4044 Plastomer for Extrusion Coating and Cast Film Applications  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade; Polyethylene (PE)

Material Notes: Data provided by the manufacturer, Exxon Chemical.

An ethylene-based hexene plastomer produced using Exxon Chemical's EXXPOL technology. It is designed for monolayer and coextrusion coating industrial fill applications and cast films. Data for film properties below based on 0.8 mil film.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccExxon Method
Thickness 0.800 mil
Melt Flow 16.5 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 4.70 MPaASTM D882
Film Tensile Strength at Yield, TD 4.10 MPaASTM D882
Film Elongation at Break, MD 480 %ASTM D882
Film Elongation at Break, TD 700 %ASTM D882
Secant Modulus, MD 0.0644 GPaASTM D882
Secant Modulus, TD 0.0596 GPaASTM D882
Instrumented Impact Total Energy 1.00 J
@Temperature 23.0 °C
ASTM D-4272
Elmendorf Tear Strength, MD 310 g/milASTM D1922
Dart Drop 1850 g/milF50; ASTM D-1709
Film Tensile Strength at Break, MD 55.4 MPaASTM D882
Film Tensile Strength at Break, TD 44.1 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 89.0 °CExxon Method
 
Optical PropertiesOriginal ValueComments
Haze 0.10 %ASTM D1003
Gloss 97 %45°, ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exxtra™ Seal POP 3500 Plastomer for Cast Film Applications
ExxonMobil EXXELOR™ VA 1840 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXXELOR™ VA 1801 Maleic anhydride functionalized elastomeric ethylene copolymer
ExxonMobil EXACT™ 4150 Plastomer
ExxonMobil EXACT™ 4011 Plastomer for Cast Film

PEXCIC / 38032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.