MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NuSil MED-4011 Silicone, Low Consistency Elastomer - Restricted Medical Use
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provides other unique properties.

Important Properties: LCEs lend themselves to applications that require a pourable, selfleveling silicone. Applications include: encapsulating a device, backfilling a void, potting an electronic component that cannot withstand exposure to high heat, or prototyping a mold. Features of low consistency elastomers may include the following:

  • Optically clear
  • Self-leveling
  • Low and high temperature cure
  • Low viscosity
  • Easy to process
Comments: Flowable

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Viscosity 1600 cPB
 114000 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25Typical
 25 - 35Certified
Tensile Strength at Break 4.70 MPaTypical
Elongation at Break 350 %Certified
 530 %Typical
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 150 °C
Post
 3.00 min
@Temperature 150 °C
 
Descriptive Properties
Mix Ratio10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED-4211 Low Consistency Elastomer - Unrestricted Medical Use

PNUSIL426 / 142150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.