MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beologic Beosmart ASA INJ550 Injection Molding
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Main properties: UV resistant, moderate stiffness, good impact. Applications: general purpose, industrial goods, furniture, household, non-food packaging

Information provided by Beologic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183-1
Melt Flow 13 g/10 min
@Load 10.0 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 49.1 MPaISO 527-1
Elongation at Break 5.3 %ISO 527-1
Tensile Modulus 2140 MPaISO 527-1
Flexural Modulus 2246 MPaISO 178
Charpy Impact, Notched 15.1 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CISO 75-1 (B)
Vicat Softening Point 94.0 °CB120; ISO 306
 
Descriptive Properties
Beologic Article Number9807000550
BiodegradableyesEN13432
Carbon footprint (kg CO2 eq/kg)0.97PAS 2050
Recycled content (%)>35
Renewable contentyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEOL9873 / 314159

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.