MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical BRE-58 Solid Brominated Epoxy Resin Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) is the most innovative fine chemical manufacturer in Taiwan. GYC Group owns the strongest R&D team and abundant functional product line. BRE series are Br content solid epoxy resin flame retardant which are accomplished by the reaction of di-glycigy of TBBA and TBBA. Two groups are epoxide.

Advantages:

  • Better heat stability than TBBA.
  • Be reacted with amine, amide, carboxylic acid, inorganic acid, anhydride which are better than conventional additives of flame retardant and TBBA powder.
  • Heat resistant
  • Good adhesion
  • Good chemical resistance
  • Dimension stability
  • Better elevated temperature performance.
Applications: Flame retardant for PBT, PET, thermoplastic resin

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Softening Point 58.0 - 64.0 °C136 - 147 °F
 
Descriptive Properties
Composition340-390 g/eqEEW

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN192 / 266500

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.