MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals SURPASS® RMs539-U sLLDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes:

Octene copolymer

Features:

  • Exceptional low temperature impact properties
  • Outstanding stiffness
  • Broad processing window
  • Low viscosity for exceptional processability, shorter cycle times, and energy savings
  • Superior whiteness for improved part appearance
  • Easy mold release
  • NSF listed for Standards #24, 51, 61
  • UL94 HB

Additives:

  • Processing antioxidant
  • UV stabilizers (estimated UV resistance >UV16)

Applications:

  • OEM custom and proprietary components
  • Recreational and leisure equipment
  • Containers, septic tanks and fish boxes
  • Marine products

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: SURPASS RMs539-U(UG) resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitations that it may contact food only at temperatures of 212°F and below (21 CFR 176.170(c), Table 2, conditions of use B–H), and that finished articles must have a volume greater than 5 gal. U.S. (18.9 L) when contacting fatty foods (21 CFR 176.170(c), Table 1, food types III, IV-A, V, VII-A and IX).

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D 792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50, Condition A & B; ASTM D 1693
Melt Index of Compound 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa
@Thickness 1.91 mm
Type IV specimen, 2" (50.8 mm) per minute speed test; ASTM D 638
Elongation at Yield 13 %
@Thickness 1.91 mm
Type IV Specimen, 2" (50.8 mm) per minute test speed; ASTM D 638
Flexural Modulus 780 MPa
@Strain 1 %
ASTM D 790
Impact Test 73.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 230 J
@Thickness 6.35 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °C(DSC)
Heat Distortion Temperature 42.0 °C
@Pressure 1.82 MPa
ASTM D 648
 60.0 °C
@Pressure 0.455 MPa
ASTM D 648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LLP8555.25 Rotational Molding Resin
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE
NOVA Chemicals SURPASS® RMs539-UG sLLDPE Rotational Molding Resin
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding)
Nexeo® HIVAL® 106033 Linear Low Density Polyethylene

PNOVB104 / 194712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.