MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis RE216CF Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RE216CF is a random copolymer suitable for the manufacturing of unoriented films for metallization. RE216CF is recommended for Lamination films, Metallisable Cast film, Stationary films, and Blending components.

Former trade name for this product was BorPure™.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.910 g/ccISO 1183
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 550 - 750 %ISO 527-3
Tensile Modulus 400 - 500 MPaMD/TD; ISO 527-3
Flexural Modulus 800 MPaISO 178
Dart Drop, Total Energy 20.0 J
@Thickness 0.0500 mm
1150N; ISO 7765-2
Coefficient of Friction <= 0.50film to film; ISO 8295
Film Tensile Strength at Break, MD 30.0 - 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 25.0 - 45.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 142 - 148 °CDSC; ISO 3146
Vicat Softening Point 130 °C
@Load 1.02 kg
A50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %ASTM D1003
Gloss >= 120 %20° of arc; ASTM D2457
 
Component Elements PropertiesOriginal ValueComments
SiO2 0.18 %Antiblock; Borealis Method
 
Descriptive Properties
Metal Adhesion (tape test)ExcellentBorealis Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis RD208CF Polypropylene Random Copolymer
Borealis BorPURE™ RD266CF Polypropylene Random Copolymer
Borealis Borclear™ RE936CF Polypropylene Random Copolymer
Borealis Bormed™ RB801CF Polypropylene Random Copolymer
Borealis RB501BF Polypropylene Copolymer

PBOREA346 / 108606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.