MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel™ ETFE HT-2202HS Special purpose fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: Tefzel™ ETFE HT-2202HS is a special-purpose fluoroplastic resin available in 2.5-mm (0.1-in) pellets. Tefzel™ ETFE HT-2202HS is a high flow modified ETFE resin designed to promote adhesion between polyamide resins and ETFE resins. Tefzel™ ETFE HT-2202HS and the other Tefzel™ fluoroplastics are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high performance resins that can be processed at relatively high rates compared with other fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. Tefzel™ ETFE HT-2202HS is an easy-to-process adhesive material. Tefzel™ ETFE HT-2202HS is inert to most solvents and chemicals, hydrolytically stable, and weather-resistant. Applications: electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, multilayer tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Water Absorption 0.0070 %
@Time 86400 sec
ASTM D570
Melt Flow 30 g/10 minASTM D3159
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 35.0 MPaASTM D3159
Elongation at Break 250 %ASTM D1457
Elongation, Ultimate 250 %ASTM D3159
Flexural Modulus 1.00 GPaASTM D790
Flex Crack Resistance 10000 - 27000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBASTM D256
Coefficient of Friction 0.030 - 0.40ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+15 ohmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 79.0 kV/mm
@Thickness 0.100 mm
film; ASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 122 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 250 - 280 °CNominal; ASTM D3159
Flammability, UL94 V-0
Oxygen Index 30 - 32 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Heat of Combustion13.7 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceExcellent
Weather Resistance (years unaffected)15Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8781 / 268707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.