MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Entec HYBOOST® 255 Masterbatch, LLDPE
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: HyBoost-255 provides mid and longer term reduction in coefficient of friction and typically reaches its’ optimum reduction in COF after 6-8 days. HyBoost-255 is a 5% active formulation providing a more economical and easily handled use rate.
Description: Masterbatch concentrate based on LLDPE with 5% Erucamide Slip blend.
Applications: HyBoost-255 main use is in addition to film to reduce coefficient of friction (COF) and improve the ease and speed of process. HyBoost-255 also has shown some property enhancement compared to film with no additive. Use rate will vary dependent upon polymer structure, impact on printing and process details.

Availability: North America

Agency Ratings: FDA Food Contact

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Additive Concentration0.05
Additives CategoryMasterbatch -- Slip Agent/Lubricant/Mold Release/Processing Aid -- Fatty Amide
Carrier ResinPolyethylene or ethylene-olefin copolymer (PE)
Chemical DescriptionErucamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB690 / 311383

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.