MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Dense Fused Silica Pre-Cast Shapes
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, copper, zinc, brass, steel, glass, and aerospace applications. It is durable and resists breakage during handling and cleaning. Components made from Pyrocast Dense Fused Silica resist cracking due to the material's low thermal expansion.

Applications

  • Spouts
  • Control pins
  • Mounting seats (inserts)
  • Pre-cast trough tiles
  • Thimbles
  • Wear plates
  • Trough dams

Advantages

  • Resistant to thermal shock
  • Superior strength
  • Low thermal expansion
  • Economically priced
  • Resistant to surface corrosion
  • Able to rapidly cycle
  • Computer controlled firing
  • Superior material consistency

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 - 1.95 g/cc0.0636 - 0.0704 lb/in³
Open Porosity 8.0 - 10 %8.0 - 10 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0170 - 0.0200 GPa2.47 - 2.90 ksi
Compressive Strength 48.0 - 51.0 MPa6960 - 7400 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.500 - 0.700 µm/m-°C
@Temperature 20.0 °C
0.278 - 0.389 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.800 W/m-K
@Temperature 13.0 °C
5.55 BTU-in/hr-ft²-°F
@Temperature 55.4 °F
Maximum Service Temperature, Air 1090 °C1990 °FSustained
 1650 °C3000 °FPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ceradyne Thermo-Sil® HS Fused Silica
Sharadaa Ceramics Sharada RFC-Fused Silica Gel Bonded Castables
Morgan Advanced Ceramics Fused Silica Cast Thermal Ceramic
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement
Pyrotek SF-50 Foamed Fused Silica Insulation Board

CPYRO066 / 1805

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.