The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant HC compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements. Property data measured on molded test bars: Dry as Molded |