MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 381 Epoxy Prepreg with S2 Uni-glass 284FAW Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 381 epoxy prepreg is an epoxy prepreg that offers a 250°F (121°C) curing system with high 180°F (82°C)/wet mechanical properties yet has the excellent fatigue and durability necessary for primary structure applications.

Features & Benefits:

  • Excellent 180°F (82°C)/wet properties
  • Service temperature to 220°F (104°C)
  • Three- to four-fold increases in fatigue life compared to perhaps all conventional 250°F (121°C) curing epoxy prepregs. This increase is the result of a 10 – 15% higher strain endurance limit.
  • Inherent toughness provides good durability and compression after impact performance
  • Low moisture absorption
  • Excellent for vacuum pressure/oven processing
Applications:
  • Primary and secondary structural aircraft parts requiring 180°F (82°C)/wet retention of properties and/or excellent fatigue behavior
  • Components that require good durability and/or low processing temperatures
  • Helicopter rotor blades
  • Rotating or cycled components
  • Co-cured aluminum assemblies/parts
  • Doublers
  • Propellers
  • Composite repair

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4100 psi
@Temperature 71.0 °C
90°; SACMA SRM-4
 7500 psi
@Temperature 82.0 °C
90°, dry; SACMA SRM-4
 8200 psi
@Temperature 22.0 °C
90°, dry; SACMA SRM-4
 9100 psi
@Temperature -54.0 °C
90°, dry; SACMA SRM-4
 113000 psi
@Temperature 71.0 °C
0°, wet; SACMA SRM-4
 208000 psi
@Temperature 82.0 °C
0°, dry; SACMA SRM-4
 236000 psi
@Temperature -54.0 °C
0°, dry; SACMA SRM-4
 243000 psi
@Temperature 22.0 °C
0°, dry; SACMA SRM-4
Elongation at Break 1.65 %
@Temperature 71.0 °C
0°, wet; SACMA SRM-4
 3.15 %
@Temperature 82.0 °C
0°, dry; SACMA SRM-4
 3.41 %
@Temperature -54.0 °C
0°, dry; SACMA SRM-4
 3.58 %
@Temperature 22.0 °C
0°, dry; SACMA SRM-4
Tensile Modulus 7.40 GPa
@Temperature 71.0 °C
90°, wet; SACMA SRM-4
 11.1 GPa
@Temperature 82.0 °C
90°; SACMA SRM-4
 12.1 GPa
@Temperature 22.0 °C
90°, dry; SACMA SRM-4
 14.5 GPa
@Temperature -54.0 °C
90°, dry; SACMA SRM-4
 45.6 GPa
@Temperature 82.0 °C
0°, dry; SACMA SRM-4
 46.7 GPa
@Temperature 22.0 °C
0°, dry; SACMA SRM-4
 47.3 GPa
@Temperature 71.0 °C
0°, wet; SACMA SRM-4
 47.8 GPa
@Temperature -54.0 °C
0°, dry; SACMA SRM-4
Poissons Ratio 0.55
@Temperature -54.0 °C
dry
 0.60
@Temperature 22.0 °C
dry
 0.69
@Temperature 82.0 °C
dry
 0.72
@Temperature 71.0 °C
wet
Shear Modulus 1.20 GPa
@Temperature 14.0 °C
In-plane, SACMA SRM-7, wet
 2.50 GPa
@Temperature 82.0 °C
In-plane, SACMA SRM-7, wet
 3.00 GPa
@Temperature 121 °C
In-plane, SACMA SRM-7, dry
 3.20 GPa
@Temperature 71.0 °C
In-plane, SACMA SRM-7, wet
 3.80 GPa
@Temperature 82.0 °C
In-plane, SACMA SRM-7, dry
 4.80 GPa
@Temperature 22.0 °C
In-plane, SACMA SRM-7, dry
 6.10 GPa
@Temperature -54.0 °C
In-plane, SACMA SRM-7, dry
Shear Strength 7200 psi
@Temperature 71.0 °C
0° Short Beam, wet; SACMA SRM-8
 7600 psi
@Temperature 14.0 °C
In-plane, wet; SACMA SRM-7
 9000 psi
@Temperature 82.0 °C
0° Short Beam, dry; SACMA SRM-8
 9200 psi
@Temperature 82.0 °C
In-plane, wet; SACMA SRM-7
 9500 psi
@Temperature 71.0 °C
In-plane, wet; SACMA SRM-7
 9900 psi
@Temperature 121 °C
In-plane, dry; SACMA SRM-7
 11800 psi
@Temperature 82.0 °C
In-plane, dry; SACMA SRM-7
 12300 psi
@Temperature 22.0 °C
0° Short Beam, dry; SACMA SRM-8
 13600 psi
@Temperature -54.0 °C
In-plane, dry; SACMA SRM-7
 14300 psi
@Temperature 22.0 °C
In-plane, dry; SACMA SRM-7
 15800 psi
@Temperature -54.0 °C
0° Short Beam, dry; SACMA SRM-8
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °F
 
Processing PropertiesOriginal ValueComments
Gel Time 5.00 - 8.00 min
@Temperature 121 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 381 Epoxy Prepreg with S2 Uni-glass and 111FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Graphite Fabric and 195FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Uni-graphite and 145FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with IM7 Uni-graphite and 148FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy

PCYTED078_5 / 192658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.