MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HE4873 High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: HE4873 is a fully formulated compound for physical foamed data cable insulation. HE4873 is a high-density polyethylene compound containing blowing agent for the production of foam or foam-skin insulation. Applications: HE4873 is designed to use as physically foamed insulation for data cables. HE4873 meets the following material classification: ISO 1872-PE, KEGHN, 45-D045, and ASTM D1248 Type III, Class A, Category 3, Grade E1, E3. The following cable material standards are met by HE4873: EN 50290-2-23. Cables manufactured with HE4873 using sound extrusion practice normally comply with the following cable product standards: IEC 61156 and EN 50288.

Former trade name for this product was Borcell™.

Information provided by Borealis AG

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccISO 1872-2/ISO 1183
Melt Flow 3.8 g/10 min
@Load 5.00 kg,
Temperature 140 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 611 second; ISO 868
Tensile Strength at Break 23.0 MPaISO 527
Elongation at Break 600 %ISO 527
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Zone 1 160 °C
Zone 2 170 °C
Zone 3 215 °C
Zone 4 205 °C
Zone 5 210 °C
Die Temperature 220 °C
Head Temperature 220 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables
Borealis BL2631 High Density Polyethylene
Borealis BL2571 High Density Polyethylene
Borealis BL1481 High Density Polyethylene
Borealis CG8410 High Density Polyethylene

PBOREA359 / 108619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.