MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 850 Premium Sealing Tape
Categories: Polymer; Tape; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Chesterton® 850 Premium Sealing Tape is a high density, moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually any thread sealing tape on the market today. Chesterton 850 Premium Sealing Tape is chemically inert and seals most types of threaded metal and plastic pipes and bots. It is nonreactive with steam, water, air fuels, refrigerants, acids, alkalies, all solvents, and gases including hydrogen, oxygen, ammonia, propane, butane, and nitrogen. For nitric or mixed acid services, factory should be consulted. Chesterton 850 Premium Sealing Tape is non-hardening and stays pliable without the breakage seen in other PTFE containing tapes. It places a slippery layer of PTFE between mated threads which remains flexible and resists vibration. Connections that might otherwise be destroyed are saved for reuse as tape eases disassembly. Slippage is minimized during application as deep penetration for threads is possible with the soft malleable tape. Joints can be adjusted 90° or more without a leak. Chesterton 850 Premium Sealing Tape is packaged in rugged easy-to carry- spools which protect the tape of dirt and contamination

Features:

  • UL Listed - US Canada
  • Meets MIL-T-27730A
  • Meets USDA requirements for incidental food contact
  • Conforms to FDA21CFR 177.1615
  • Acceptable to oxygen use
  • Non-aging
  • Non-Hardening
  • High density
  • Chemically resistant

Benefits:

  • Stays pliable
  • Always ready to use
  • Requires fewer wraps
  • Resists tearing and breakage
  • Won't clog fuel lines.

Applications: Use Chesterton 850 Premium Sealing Tape as a non-hardening, dry thread sealant for most liquids, gases, pneumatic and hydraulic fittings. Prevents bolts and fittings from seize up to 260°C. Seals all plumbing and most industrial piping threads

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
Thickness 7.50 micronsASTM D374
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 800 psiLongitudinal; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -240 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
USDA Yes
 
Descriptive Properties
ColorWhite
Pressure Testing>2500 psi
 10000 psiHydraulic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.010" thick)
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.001" thick)
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape
Klinger Thermoseal Sealex® PTFE Tape Joint Sealant
Chemours Teflon® PTFE 65 Resin for Lubricated Paste Extrusion

PPTCHS104 / 138216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.