MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend; Nylon (Polyamide PA)

Material Notes: Triax 1185 is an ABS (Acrylonitrile Butadiene Styrene) polyamide alloy for injection molding. Features: Excellent processability, Good chemical resistance, Excellent abrasion resistance, Excellent surface appearance, UL 94HB certified.

Applications: Components for recreation vehicles, Industrial and consumer applications, Snowmobiles, ATVs, Side by sides

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D 792
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 33.7 MPaASTM D 638
Flexural Modulus 1320 MPaASTM D 790
Secant Modulus, MD 4.89 ksiASTM D 882
Izod Impact, Notched 15.0 ft-lb/in
@Temperature -18.0 °C
ASTM 256
 19.0 ft-lb/in
@Temperature 23.0 °C
ASTM 256
Falling Dart Impact 35.0 ft-lbInstrumented, total energy; ASTM D 3763
Puncture Energy 11.0 J
@Temperature -30.0 °C
Energy to Maximum Force, FM- Penetration Test
Instrumented Impact Energy at Peak 20.0 J
@Temperature 23.0 °C
Multiaxial Impact; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity
 24.0 J
@Temperature -30.0 °C
Multiaxial Impact; 0.100 in. thickness, 1.57 in. ring, 0.5 in. dart, 3.46 m/s velocity
 
Thermal PropertiesOriginal ValueComments
CTE, linear 66.0 µin/in-°FASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °Cunannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °Cunannealed; ASTM D 648
Vicat Softening Point 196 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Gloss 93 %at 60°, specular; ASTM D 523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 270 °C
Mold Temperature 38.0 - 93.0 °C
Drying Temperature 88.0 °C
@Time 7200 - 14400 sec
Do not exceed 93°C
 
Descriptive Properties
Hold Pressure30-50% of Injection Pressure, Injection Molding
Injection SpeedFastInjection Molding
Screw Compression Ratio2.5:1Injection Molding
Screw Length-to-Diameter Ratio>= 20:1Injection Molding
Screw SpeedModerate, Injection Molding
Shot Weight-to-Machine Capacity Ratio0.5-0.7Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Techmer ES Plastiblend® ABS/PA 1700
INEOS Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Conditioned)
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
INEOS Styrolution Terblend® N NM-21 XP ABS+PA (Conditioned)

PINEA936 / 107207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.