MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Categories: Polymer; Thermoset; Epoxy

Material Notes: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer’s exacting standards where higher strength at elevated temperatures are required. MC511A is certifiable to MIL-I-24768/3, Type GEB and is halogen free to meet the European restrictions.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, NEMA G-11, ASTM D709 Type IV Grade G-11, MIL-I-24768/3 GEB
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.91 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 0.100 %
@Thickness 1.57 mm
ASTM D570 Condition A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 115
@Thickness 6.35 mm
ASTM D785
Flexural Strength 37000 psi
@Thickness 1.57 mm
LengthWise; Condition E-1/150 T150
 61000 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 71500 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Izod Impact, Unnotched 14.0 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 18.0 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.5
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength 610 V/mil
@Thickness 1.57 mm
ASTM D149 Condition A
 650 V/mil
@Thickness 1.57 mm
ASTM D149 Condition D-48/50
Dielectric Breakdown 65000 V
@Thickness 1.57 mm
ASTM D149 Condition A
Dissipation Factor 0.028
@Thickness 1.57 mm,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 185 sec
@Thickness 3.17 mm
ASTM D495 Conition A
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature, Tg 180 °C
@Thickness 12.7 mm
DMA
UL RTI, Electrical 170 °CUL Bulletin 746b
UL RTI, Mechanical with Impact 180 °CUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength2200[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta NP511 Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta MC511FR Epoxy Glass Laminate Sheet, NEMA FR-5
Norplex-Micarta NP130 Epoxy Glass Laminate Sheet, NEMA FR-4

PNORPM045 / 192802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.