MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOM® LDDC PC 1000 UV 18041 WT1078-12 PC, special filler, UV stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: special filler, UV stabilized

Special Features: translucent, high light diffusion, good flow

Market Segment: Automotive, Lighting

Application Area: lighting, light transparent components, White Panel-Technology

Typical Applications: lamp covers, display elements, operating elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 19 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 66.0 MPaISO 527
Tensile Strength, Yield 66.0 MPaISO 527
Elongation at Break 70 %ISO 527
Elongation at Yield 6.0 %ISO 527
Tensile Modulus 2450 MPaISO 527
Flexural Strength 100 MPaISO 178
 76.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2450 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 11.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 124 °CISO 75-1/-2
Vicat Softening Point 142 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
 V-2
@Thickness 0.750 mm
Glow Wire Flammability Index 850 °C
@Thickness 1.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 2.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 3.00 mm
passed; DIN EN 60695
 850 °C
@Thickness 4.00 mm
passed; DIN EN 60695
 960 °C
@Thickness 3.00 mm
passed; DIN EN 60695
 960 °C
@Thickness 4.00 mm
passed; DIN EN 60695
 
Optical PropertiesOriginal ValueComments
Haze 95 %
@Thickness 1.00 mm
A,2°; ISO 13468
 95 %
@Thickness 2.00 mm
A,2°; ISO 13468
 95 %
@Thickness 3.00 mm
A,2°; ISO 13468
 95 %
@Thickness 4.00 mm
A,2°; ISO 13468
Transmission, Visible 9.8 %
@Thickness 4.00 mm
A,2°; ISO 13468
 12.9 %
@Thickness 3.00 mm
A,2°; ISO 13468
 19.6 %
@Thickness 2.00 mm
A,2°; ISO 13468
 31 %
@Thickness 1.00 mm
A,2°; ISO 13468
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 310 °CInjection molding
Mold Temperature 80.0 - 110 °CInjection molding
Drying Temperature 120 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolycarbonate
Half Power Angle57°d=1mm, A,2°
 59°d=2mm, A,2°
 61°d=3mm, A,2°
 62°d=4mm, A,2°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, UV Stabilized
Mocom (ALBIS) ALCOM® PC 740/4 UV WT1370-07LD PC, UV stabilized
Mocom (ALBIS) ALCOM® PC 730/3.1 UV WT1283-09DM PC, UV stabilized
Mocom (ALBIS) ALCOM® LIR PC 1000 UV 14099 BK1203-14 PC, UV stabilized
Mocom (ALBIS) ALCOM® LD2 PC 1000 UV 15091 GY1138-15 PC, special filler, UV stabilized

PALBIS8073 / 242132

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.