MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik MP 40 Cemented Carbide Grade for Rotary Tools  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK MP40 carbide grade is a well established, high performance cemented carbide, designed to meet the ISO P40 range of metal cutting applications.

This grade is manufactured to the most exacting specifications demanded by Sandvik through its commitment to the production and supply of the high quality tool materials required by the rotary tooling in dustry.

SANDVIK grade MP40 incorporates 11% cobalt (Co) and 77% tungsten carbide (WC), 12% cubic carbide (Ti, Ta/Nb, C).

This grade offers an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

SANDVIK grade MP40 is recommended for rotary tool applications in the ISO P40 range. It has a high resistance to mechanical and thermal wear and exhibits an excellent performance when machining a wide range of materials.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 13.12 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 90.3
Hardness, Vickers 139030
Flexural Strength 3200 MPaTransverse Rupture; ISO 3327
Compressive Strength 5400 MPa
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 11 %
WC 77 %
 
Descriptive Properties
Corrosion Resistance, 1-104
Wear Resistance, 0-105

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Extramet EMT 609 Tungsten Carbide, Ultra-Fine Grain
Tungsten Carbide, WC
Sandvik H6N Cemented Carbide for Metal Forming Applications
Poco Graphite EDM-4 EDM Graphite
Mi-Tech Metals CW80 80 Tungsten/20 Copper PM Metal Composite

NSANDV030 / 18924

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.