MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
Categories: Fluid

Material Notes: VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexible polyurethane foams for furniture, bedding, and automotive seating and padding. In addition, VORANATE™ T-80 TDI products are used in the production of elastomers, coatings, adhesives, semi-flexible foams, and carpet underlayment and backing.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Viscosity Measure 2.5 cSt
@Temperature 25.0 °C
Molecular Weight 174.2 g/mol
Vapor Pressure 0.0100 torr
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.46 J/g-°C
@Temperature 20.0 °C
 1.72 J/g-°C
@Temperature 100 °C
Melting Point 14.0 °C
Boiling Point 120 °C10 mm Hg
 250 °C760 mm Hg
Decomposition Temperature 287 °C
Flash Point 126 °CPensky Martens closed cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5662

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANOL™ 4701 Polyether Polyol
Dow BETAFOAM™ 87124 Polyether / Polyol Blend

PDOW1088 / 30292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.