MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SARAN™ 560 CX Vapor Retarder Tape  (discontinued **)
Categories: Polymer; Adhesive

Material Notes: SARAN™ 560 CX Vapor Retarder Tape is composed of durable, flexible polyvinylidene chloride (PVDC) coated with a pressure sensitive acrylic adhesive designed for effective and long-lasting adhesion to a variety of substrates. Designed specifically for high vapor drive applications, SARAN 560 CX Tape conforms easily to fittings, elbows and joints, creating a tight, water-resistant seal and protecting these vulnerable areas from moisture intrusion and energy loss. A permeance rating of 0.01 perms meets or exceeds the strictest industry requirements for vapor retarders in cold service.

Applications: SARAN™ 560 CX Vapor Retarder Tape is used to wrap elbows and fittings in many high-moisture environments over a wide temperature range. The high performance tape is also used to seal butt joints and seams in the vapor retarder system. Typical applications for SARAN 560 CX Tape include:

  • Food and beverage facilities
  • Chilled water piping and HVAC systems
  • Transport pipelines
  • Chemical condensation tanks
  • Cold storage systems
  • Refrigerated transport
  • Pharmaceutical plants
  • Petrochemical plants
  • Cryogenic systems, including liquefied natural gas (LNG)

SK Global Chemical has purchased the SARAN® resin business from Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.50 milAdhesive; ASTM D3652
 6.00 milBacking; ASTM D374
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 psiASTM D3759
Elongation at Break 145 %ASTM D3759
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
Flame Spread Index 0.00ASTM E84
 
Descriptive Properties
Adhesion30 oz/into Steel, Initial, ASTM D3330
 50 oz/into Steel, after 3 days at 72°, ASTM D3330
 55 oz/into SARAN™ Film, Initial, ASTM D3330
 60 oz/into SARAN™ Film, after 3 days at 72°, ASTM D3330
ColorWhite
Permeance0.01ASTM E96
Surface Burning Characteristics5Smoke Developed, ASTM E84

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SARAN™ 560-CX Vapor Retarder Film
SK Chemicals Saran® 560 Vapor Retarder Film
SK Chemicals Saran® 560 Clear Plastic Barrier Film
Tin, Sn
Elliott Company ELFOAM® P200 Polyisocyanurate Foam

PITWZ004 / 187070

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.