MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem IC32 LLDPE Injection Molding Polyethylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: IC32 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding. It offers good fluidity, excellent flexibility and tenacity, and low warpage. It contains special antioxidant additives. This resin has been specifically developed for lids molding injection, house appliances, and masterbatch production. IC32 resin has been developed to be used in injection molding in similar conditions to other linear low-density polyethylene of similar fluidity. Recommended temperature profile: 150 to 200ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM-D729
ESCR 10% Igepal® 0.80 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 29 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPaASTM-D638
Tensile Strength, Yield 12.0 MPaASTM-D638
Elongation at Break 250 %ASTM-D638
Modulus of Rigidity 0.320 GPaASTM-D747
Flexural Modulus, 1% Secant 370 MPaASTM-D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °C
@Load 1.02 kg
ASTM-D1525
Brittleness Temperature <= -70.0 °CASTM-D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem H 103 Injection Molding Polypropylene
Braskem PB 608 LDPE Injection Molding Polyethylene
Braskem LL318 LLDPE Linear Low Density Extrusion Polyethylene
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin

PBRAS908 / 106754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.