MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen RP220M Polypropylene Copolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Moplen RP220M is a controlled rheology medium modified propylene random copolymer for manufacturing high transparent cast films. It contains no slip or antiblocking agents. It offers good processability, excellent clarity and gloss and exhibits very good heat weldability. Main applications are packaging of foodstuffs, packaging of stationary, shirts and hosiery. It is also suitable for production of stationary folders. Moplen RP220M is suitable for food contact. Applications: Food Packaging Film, Stationery Film, Textile Packaging Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 26.0 MPaISO 527-1,-2
Tensile Strength, Yield 23.0 MPaISO 527-1,-2
Elongation at Break >= 500 %ISO 527-1,-2
Elongation at Yield 12 %ISO 527-1,-2
Flexural Modulus 700 MPaISO 178
Charpy Impact, Notched 2.50 kJ/m²
@Temperature 0.000 °C
Type 1, Edgewise, Notch A; ISO 179
 10.0 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 125 °CA50, 50C/h, 10N; ISO 306
 
Descriptive Properties
Processing MethodCast film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Novolen® 1125 N Polypropylene
Westlake HM 5004 High Density Polyethylene
BASF Novolen® 2500 H Polypropylene
BASF Novolen® 2900 H Polypropylene
BASF Novolen® 3200 H Polypropylene

PEQT9082 / 220713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.