MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtra™ Soft EMA2022 Blown Ethylene Methyl Acrylate, Film Grade
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Film Grade

Material Notes: Exxtra™ Soft EMA2022 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elastic film with good handling characteristics without additional additives. It can produce film under 1.0 mil thickness.

Availability: Latin America, North America

Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes

Applications: Disposable Gloves, Hospital Drapes, Upholstery Film

Information provided by ExxonMobil.

Key Words: Optema™ TC 111 Blown
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.943 g/ccASTM D1505
Methyl Acrylate Content 21.5 %ExxonMobil Method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 380 %ASTM D882
Film Elongation at Break, TD 640 %ASTM D882
Secant Modulus, MD 5.80 ksiASTM D882
Secant Modulus, TD 4.90 ksiASTM D882
Elmendorf Tear Strength MD 40 gASTM D1922
Elmendorf Tear Strength TD 380 gASTM D1922
Dart Drop Test 480 gASTM D1709A
Film Tensile Strength at Break, MD 3200 psiASTM D882
Film Tensile Strength at Break, TD 3200 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 176 °FPeak; ExxonMobil Method
Vicat Softening Point 124 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 14 %ASTM D1003
Gloss 37 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98895 / 238277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.