MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8115 sec; ASTM D2240
Tensile Strength, Yield 50.5 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2830 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 104 MPaASTM D790
Flexural Modulus 2900 MPaASTM D790
Izod Impact, Notched 51.0 J/m
@Thickness 3.18 mm,
Temperature -40.0 °C
Compression Molded; ASTM D256A
Dart Drop Total Energy 62.3 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 133 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 193 °C
 
Descriptive Properties
Agency RatingsNSF 51
 NSF Type I
Ease of SizingGood
FeaturesGood Chemical Resistance
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification12454ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesPiping

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40

PH0POL0796 / 145365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.