MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Pressure Seal 19511 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Compound 19511 is a 50 durometer salmon colored general purpose Silicone elastomer. It exhibits good resistance to heat and compression set and will remain non brittle at very low temperatures.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 GE 504 A19 B37 EO16 EO36 F19 EA14 G11; 4 GE 507 A19 B37 EO16 EO36 F19 EA14; 5 GE 507 A19 B37 EO16 EO36 F19 EA14
ZZ-R-765 Class 2a & 2b Grade 50
A-A-59588 Class 2a & 2b Grade 50
AMS 3302

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
 33
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #3
 47
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 48
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 52
@Treatment Temp. 100 °C,
Time 252000 sec
Distilled water aged
 55
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
 56
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
Tensile Strength 939 psi
 860.1 psi
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 1004.7 psi
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
 1017.9 psi
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
 1018.8 psi
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
Elongation, Ultimate 341 %
 295 %
@Treatment Temp. 150 °C,
Time 252000 sec
ASTM Oil #1
 312.4 %
@Treatment Temp. 175 °C,
Time 252000 sec
ASTM Oil #1
 354 %
@Treatment Temp. 225 °C,
Time 252000 sec
Heat Aged
 366.9 %
@Treatment Temp. 200 °C,
Time 252000 sec
Heat Aged
100% Modulus 220 psi
Tear Strength 49.0 pliDie B
 79.0 pliDie C
Compression Set 6.3 %
@Treatment Temp. 175 °C,
Time 79200 sec
Plied
 8.2 %
@Treatment Temp. 150 °C,
Time 252000 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -103 °F
Shrinkage 0.50 %
@Treatment Temp. 100 °C,
Time 252000 sec
Volume, Distilled water aged
 2.6 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 4.8 %
@Treatment Temp. 175 °C,
Time 252000 sec
Volume, ASTM Oil #1
 44.6 %
@Treatment Temp. 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 
Descriptive Properties
ColorSalmon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL162 / 318372

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.