MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Pyranin 120 Percent Brilliant yellow dye
Categories: Other Engineering Material

Material Notes: General Brilliant yellow dye with strong greenish fluorescence in alkaline solutions for ink, detergent and tracing applications; Complies with EN 71-3 and 71-9 (toy safety regulations); Complies with purity criteria for colorants used in cosmetics; Complies with FDA specifications for D&C Green 8

Applications:

  • Office supplies (water-based inks, yellow highlighters)
  • Alkaline cleaning agents, shampoos, soaps
  • Tracing agent in water and heating systems

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 4.0 - 5.010% in water
 3.0
@Wavelength 290 nm
 3.0
@Wavelength 520 nm
 9.0
@Wavelength 450 nm
 9.0
@Wavelength 520 nm
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
AppearanceYellow powder
Content<15%Salt content
Specifications±5%Color strength tolerance
 1Lightfastness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8920 / 209312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.