MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NUDEC® PET Polyester Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Brightness and transparency make NUDEC®PET the ideal product for advertising elements. It also possesses high resistance to the chemical attack of acid rain, diesel engine exhaust fumes and air with a certain amount of salinity, which makes it very useful outside in the UV version. NUDEC®PET plastic sheets have a good impact strength and fire resistance. Along these lines, they have obtained B1 certification of the German DIN4102-1 and M2 certification French NFP-507 standard. On order, patterned PET sheets can be manufactured. These sheets are often used as light diffusers or bathroom screens, among other applications. Sheet properties: Excellent transparency and brightness. High resistance to chemical products. High impact strength and resistance to breakage. Thermoformable, do not require any pre-drying.Excellent fire resistance. Low generation of non-toxic smoke. Recyclable, respectful of the environment, completely combustible, without any emission of toxic substances that contaminate landfills. More advantages: Anti-reflective. Impact-resistant. Lightweight and good rigidity. Easy handling. Colors are maintained bright.

Information provided by NUDEC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 117 MPaISO 2039
Tensile Strength, Yield 59.0 MPaISO 527
Tensile Modulus 2.42 GPaISO 527
Flexural Strength 86.0 MPaISO 178
Charpy Impact Unnotched NBISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear >= 60.0 µm/m-°CISO 75-2
Maximum Service Temperature, Air 60.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CHDT B; ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °CHDT A
Vicat Softening Point 75.0 °C
@Load 5.10 kg
ISO 306
 79.0 °C
@Load 1.02 kg
ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.576ASTM D-542
Transmission, Visible 89 %ASTM D-1003
 
Descriptive Properties
Chemical ResistanceAcetic Acidsatisfactory
 Acetoneunsatisfactory
 Ammoniaunsatisfactory
 Detergentssatisfactory
 Ethanolsatisfactory
 Gasolinesatisfactory
 Glycerinsatisfactory
 Methanolregular
 Mineral oilsatisfactory
 Toluenesatisfactory
 Turpentinesatisfactory
 vegetable oilsatisfactory
 Watersatisfactory
FlammabilityFrance, NFP 92-507, M2
 Germany, DIN 4102-1, B1
 Great Britain, BS 476: Part 7, IY
 Italy, UNI 9177, class 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Peripor® 300 Expandable Polystyrene
NUDEC® PETg (PET modified with CHDM) Sheet
NUDEC® SANuv Acrylonitrile - Styrene Sheet
Overview of materials for Polypropylene, Molded
PolyMirae Moplen EP3307 High Impact Polypropylene Copolymer

PNUDEC991 / 192057

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.