MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NYCOA 1838 Copolymer Nylon Alloy
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: good impact resistant molding and extrusion grade

Information provided by NYCOA, Inc.

Key Words: PA 6, Polyamide 6, Nylon 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
Water Absorption 1.2 %1.2 %ASTM D570
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 54.0 MPa7830 psiASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Flexural Yield Strength 17.0 MPa2470 psiASTM D790
Flexural Modulus 1.25 GPa181 ksiASTM D790
Izod Impact, Notched 3.33 J/cm6.24 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 209 °C408 °FASTM D789
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 °C482 °F
Rear Barrel Temperature 210 °C410 °F
Middle Barrel Temperature 230 °C446 °F
Front Barrel Temperature 250 °C482 °F
Nozzle Temperature 250 °C482 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 76.0 °C169 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6)
Avient Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12)
LATI LATAMID 68 H2 G/30 30% Glass Fiber, Heat-Stabilized Nylon 66 Copolymer (Pac)
LNP Konduit® ITF-212-11 Polyamide 6/12 Copolymer
NYCOA 1595 HS Impact Modified, Medium Viscosity Nylon 6 Resin

PNYCOA10 / 55556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.