MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC PEEK CW50 PL S0002 natural - plate Polyetheretherketone, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Fillers: carbon fibers

Main features:

  • excellent chemical resistance
  • low coefficient of thermal expansion
  • continuous service temperature up to 260 °C
  • very high stiffness
  • very high strength appearance
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³
Filler Content 50.0 %50.0 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 713 MPa103000 psiISO 527-4
Tensile Modulus 59.0 GPa8560 ksiISO 527-4
Flexural Strength 866 MPa126000 psiISO 14125
Flexural Modulus 55.0 GPa7980 ksiISO 14125
Compressive Strength 645 MPa93500 psiISO 14126
Shear Strength 65.0 MPa9430 psiinterlaminar; ISO 14130
 137 MPa19900 psiinterplanar; ISO 14129
Charpy Impact, Notched 6.55 J/cm²31.2 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 µm/m-°C2.78 µin/in-°Fin 0° and 90° direction
Melting Point 343 °C649 °F
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Glass Transition Temp, Tg 143 °C289 °F
 
Processing PropertiesMetricEnglishComments
Drying Temperature 150 °C302 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
Areal weight finished product344 g/m²
Colornatural
Fiber architectureTwill 2/2
Fiber areal weight200 g/m²
Fiber orientation0-90°
Fiber typeCarbon HT 3k
Material widths625x525 mm
ply thickness (consolidated)1-95 mm
Resin weight content0.419

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN506 / 287730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.