MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 390 Cutting Oil
Categories: Fluid

Material Notes: Description: Chesterton® 390 Cutting Oil is a heavy duty, multi-purpose cutting fluid designed to provide maximum tool life and superior parts finish in severe applications. It is a highly reinforced lubricant for faster, easier cutting of hard or soft metals. Maximum lubricity means less wear on tool cutting edges and less down time, cleaner cuts and fewer rejects. The high viscosity oil clings to drills, taps, bores etc. and will provide maximum friction reduction especially when the tool is buried deep within a metal substrate. The convenient aerosol package can be applied at any angle for flat or vertical overhead work. The clinging foam means no drip and no waste. Difficult applications such as the internal threading of pipes is facilitated as 390 Cutting Oil can be easily sprayed into such normally hard to lubricate areas. Many users report that an aerosol can of 390 Cutting Oil goes as far as a gallon of ordinary cutting oil because it is directed at the cutting area and stays there.

Features:

  • Superior extreme pressure capabilities
  • Excellent part finish
  • Clings to vertical and overhead surfaces
  • Cleaner cuts
  • Protects from rust
  • No unpleasant odor
  • NSF H2, P1 – Registration number 134014 (bulk) and 134947 (aerosol)

Applications: Lubricant for all types of metal cutting and forming. Use for broaching, deep drilling, sawing, reaming, milling, tapping, hack sawing, boring, countersinking. Excellent parts finish on cast and wrought iron, black steel, Alloy 20, Hastelloy, Inconel, and other Stainless and High Carbon Steels.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
Viscosity Measure 32 cSt
@Temperature 40.0 °C
ASTM D445, DIN 51 361
 
Thermal PropertiesOriginal ValueComments
Pour Point -18.0 °CASTM D97, ISO 3016
Flash Point 170 °CASTM D93, DIN 51 755
 
Descriptive Properties
AppearanceAmber, Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlson C 625 Nickel-Chromium-Molybdenum Alloy
Chesterton 389 Synthetic Tapping Compound
Haynes Hastelloy® B-3® alloy, 0% cold work
Haynes Hastelloy® G-30® alloy, 30% cold rolled
MetalTek MTEK N-7M Cast UNS N30007 Severe Corrosion and Heat Resistant Alloy

PPTCHS115 / 138227

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.