MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 6225 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Low viscosity, heat curing silicon rubber composition for coating applications. It is supplied without crosslinker and catalyst to open wide process flexibility by customized adjustment of catalyst and crosslinker quantities. It can be cured at high temperatures within short time.

Application: ELASTOSIL® R 6225 TRANSPARENT may be used for applications which require high or low temperatures resistant, flexible coating. A typical application in the automotive industry is the final coating ("top coat") of fiber cylinder head gaskets.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDIN 51757
Brookfield Viscosity 2500 cPdynamic, after mixing
 3000 cPdynamic
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45cured; DIN 53505
Tensile Strength at Break 5.00 MPacured; DIN 53504
Elongation at Break 125 %cured; DIN 53504
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 5.00 min
@Treatment Temp. 180 °C
 5.00 - 10.0 min
@Treatment Temp. 150 °C
Gel Time 30.0 min
@Temperature 100 °C
 
Descriptive Properties
Appearancecolorless
 transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 32980R015 0.015" (0.381 mm) Uncured Silicon Rubber on Polyester Film Carrier
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
G-10 Fiberglass Epoxy Laminate Sheet

PWACK9253 / 204782

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.