MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-16V-2.5Al, Duplex Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Duplex Annealed: 760 °C, 30 min, air cooled + 525 °C, 4 to 6 hours, air cooled. Mechanical properties reported are for Sheet of thickness 1.6 mm.

Characteristics: Metastable beta alloy, age-hardenable.

Applications: High-strength sheet for aerospace.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.65 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1110 MPaLongitudinal
 1131 MPaTransverse
Tensile Strength, Yield 1000 MPaLongitudinal
 1034 MPaTransverse
Elongation at Break 5.4 %Transverse
 6.2 %Longitudinal
Tensile Modulus 95.8 GPaLongitudinal
 97.9 GPaTransverse
Compressive Yield Strength 1044 MPaLongitudinal
 1076 MPaTransverse
Compressive Modulus 97.2 GPa
Ultimate Bearing Strength 1613 MPae/D = 1.5
 1944 MPae/D = 2.0
Bearing Yield Strength 1434 MPae/D = 1.5
 1593 MPae/D = 2.0
Shear Strength 690 MPaTransverse
 703 MPaLongitudinal
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µm/m-°C
Specific Heat Capacity 0.527 J/g-°C
Thermal Conductivity 8.70 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 %
Titanium, Ti 81.5 %
Vanadium, V 16 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3RE60 Duplex Stainless Steel, Annealed Pipe, UNS S31500
Titanium Ti-15Mo-5Zr-3Al Duplex Aged
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Solution Treated
Titanium Transage 129, Duplex Heat Treat 760/480°C
Titanium Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2), Duplex Annealed

MTB162 / 142966

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.