MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTORAN® 1900GF20 HE30018 Polyphenylene Ether, Glass/Graphite Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Glass/Graphite Reinforced

Material Notes: Modified polyphenylene ether (PPE), heat resistant, glass fiber-reinforced, suitable for K&K process. Amorphous VESTORAN® 1900GF20 HE30018 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp. Moldings of VESTORAN® 1900GF20 HE30018 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900GF20 HE30018 is resistant to aqueous alkalines and acids, certain alcohols, and glycol solutions. Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity. VESTORAN®1900GF20 HE30018 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites patented K&K process ("direct-bonding to rubber"). VESTORAN® 1900GF20 HE30018 is supplied as cylindrical granules in polyethylene packaging. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0600 %ISO 15512
Melt Flow 45 g/10 min
@Load 21.6 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 103 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 5700 MPaISO 527
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 195 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °CISO 75-1/-2
Vicat Softening Point 195 °CMethod B: 10 N, 50 K/h; ISO 306
 205 °CMethod A: 10 N, 50 K/h; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK888 / 243095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.