MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC; Vinyl Ester

Material Notes: The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compression, transfer, or injection molded.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccASTM D572
Water Absorption 0.29 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 48.0 MPa
Flexural Strength 159 MPa
Compressive Strength 145 MPa
Izod Impact, Notched 5.90 J/cmedgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 15.0 kV/mmPerpendicular (ASTM D149), Short Time
Arc Resistance 187 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °Ctemperature rating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 845 30% Glass Filled Vinyl Ester
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced

PHAY04 / 45610

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.