MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TechnoCompound TechnoDur PBT/PET GF 30 Natural (9966) PBT/PET, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + PET Blend, Glass Filled

Material Notes: Our new TechnoDur PBT compound is a thermoplastic which combines great hardness, stiffness and strength. TechnoDur is easily processed due to its perfect flow behavior. The favorable sliding and wear characteristics as well as extremely high tenacity in temperatures below freezing are further advantages.

Typical Applications: TechnoDur compounds may be applied in the following areas:

  • Electrical engineering: Lamp holders, micro switches, spools, brush-holder bridges, switches, cam devices, telephone housings
  • Automobile construction: Junction boxes, petrol filters, fuel tank caps, heating, folds, headlights, car body panels, spark plug connectors
  • Household appliances: Hair care appliances, components for toasters, fondue makers, coffeemakers
  • Other: pump components, gears guide applications: slide bearings and components

Information provided by TechnoCompound

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccISO 1183
Moisture Absorption 0.130 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 0.40 %ISO 62
Viscosity Number 106.4 cm³/gISO 1628-5
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Pressure 60.0 MPa,
Temperature 260 °C
WZ 80 °C; ISO 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Pressure 60.0 MPa,
Temperature 260 °C
WZ 80 °C; ISO 2577
Melt Flow 14 g/10 min
@Load 0.00216 kg,
Temperature 265 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 220 MPa
@Load 36.5 kg
ISO 2039-1
Tensile Strength at Break 155 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
Tensile Modulus 10500 MPa1 mm/min; ISO 527
Flexural Strength 220 MPa2 mm/min; ISO 178
 210 MPa
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 9000 MPa2 mm/min; ISO 178
Flexural Strain at Break 3.0 %2 mm/min, flexural strength; ISO 178
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60251
 4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
@Thickness 1.00 mm
Short Time; IEC 60243-1
Comparative Tracking Index 250 VA; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Melting Point 220 - 255 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75
Deflection Temperature at 8.0 MPa 125 °CISO 75
Vicat Softening Point 225 °C
@Load 5.10 kg
50 °C/h; ISO 306
Flammability, UL94 HB
@Thickness 0.800 mm
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTECHNO032 / 306394

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.