MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GD 7255 High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Hostalen GD 7255 is a high density polyethylene resin used in general injection molding applications such as pallets and dust bins. Hostalen GD 7255 is available in pellet form, and exhibits high ESCR, good impact resistance, flowability and low warpage. Hostalen GD 7255 is not intended for use in medical and pharmaceutical applications. Applications: Caps & Closures, Crates, House wares, Industrial, Panels & Profiles, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccISO 1183-1
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 11 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Ball Indentation Hardness 52.0 MPaISO 2039-1
Tensile Strength, Yield 27.0 MPaISO 527-1,-2
Elongation at Yield 8.0 %ISO 527-1,-2
Tensile Modulus 1200 MPaISO 527-1,-2
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 4.50 kJ/m²
@Temperature -30.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 73.0 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °C
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
FNCT (hrs)4.5ISO 16770, 6.0 MPa, 2% Arkopal N100, 50°C
Processing Methodinjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethydco Advancene™ EM-6308-UV High Density Polyethylene Resin
LyondellBasell Hostalen GD 7255 LS High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Lupolen 5031 L HDPE, Injection Molding Grade
Celanese GUR® HOSTALLOY 731 Injection Molding Grade Polyethylene Resin
LyondellBasell Alathon® H5520 High Density Polyethylene

PEQT8482 / 220117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.