MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos J60-1700-173 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: J60-1700-173 is a high density polyethylene homopolymer. This resin is a product of Ineos' technology and is characterized by a narrow molecular weight distribution. Parts fabricated from this material exhibit excellent gloss and rigidity. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: High gloss and rigidity
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D4883
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
16 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 31.0 MPa4500 psi2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.552 GPa225.1 ksiTangent; ASTM D 790
Izod Impact, Notched 0.380 J/cm0.712 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C178 °FASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos J50-2000-119 HDPE
Ineos J50-1000-187 HDPE
Ineos J60-1700-183 HDPE
Sunoco TI6120NB Polypropylene High Impact Copolymer
Ineos J60-800-178 HDPE

PSOLKC / 68219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.