MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® IL 1351 51% BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Desmodur IL 1351 51% BA is an aromatic polyisocyanate based on toluene diisocyanate (TDI). It is used as a hardener component for fast drying, two-component polyurethane coatings.

Properties / Applications: Desmodur IL 1351 51% BA can be used in combination with certain Desmophen grades for the formulation of very fast drying systems. Such systems are used in the furniture industry, among others, where very short drying times and early sandability are required. As with any product, use of Desmodur IL 1351 51% BA in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/cc
Volatiles 47 - 51 %47 - 51 %
Viscosity 850 - 1750 cP850 - 1750 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 26.0 °C78.8 °F
 
Descriptive Properties
Color<2Iodine
Content<0.5%Monomeric TDI
 7.7-8.3%Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® IL BA Polyurethane
Covestro Desmodur® L 67 BA Polyurethane
Covestro Desmodur® IL 1351 Polyurethane
Covestro Desmodur® IL 1351 51% EA Polyurethane
Covestro Desmodur® I Polyurethane

PCOVEST0353 / 202136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.