MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 6232 Polypropylene, Blow Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade

Material Notes: Random copolymer blow molding grade for medical applications

Impact Strength -- FINA 6232 offers good impact strength, clarity and gloss.

Chemical Inertness – FINA 6232 has been formulated specifically for medical applications requiring low level extractables and low odor.

High Purity -- FINA 6232 provides optimum thermal stability for superior color and processability.

FDA -- FINA 6232 complies with all applicable FDA regulations and may be used under these provisions for food contact and packaging.

Recommended Applications -- FINA 6232 is ideal for extrusion blow molding for medical, food and other containers requiring low extractables.

Processing -- FINA 6232 resin processes on conventional blow molding equipment with typical melt temperatures of 390-450°F (199- 232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Permeability 9.40 g mil/ (m2 day)
@Temperature 37.8 °C
90% RH; ASTM E96
Density 0.900 g/ccASTM D1505
Oxygen Transmission 95.0 cc-mm/m²-24hr-atm
@Temperature 23.0 °C
cc-mm/m²-24hr-atm; ASTM D1434
Linear Mold Shrinkage 0.010 - 0.025 cm/cmASTM D955
Melt Flow 2.0 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 29.0 MPaASTM D638
Elongation at Break 10 %ASTM D638
Modulus of Elasticity 1.171 GPaASTM D638
Flexural Modulus 0.900 GPaASTM D790
Izod Impact, Notched 0.640 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 147 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 232 °Cblow molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total 7235 Polypropylene, Blow Molding Grade
Overview of materials for Polypropylene, Blow Molding Grade
Total PPR 7238 Polypropylene, Random Copolymer - Blow Molding
Total PPR 8473 Polypropylene, Film Extrusion Grade
Total PPH 3230 Polypropylene, Blow Molding Grade

PFIN39 / 38369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.