MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omnova Solutions Chemigum® P83 Nitrile Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Balanced modifier of plasticized PVC for improved properties and melt processing in the Eliokem product line. 33% bound ACN. Crosslinked polymer structure. PVC partitioning agent.

Can be used in PVC blends.

Used in automotive (interior moldings, decorative profiles/spoilers, oil and gas resistant parts), glazing gaskets, roofing membranes, flooring, footwear, cable jacketing, hoses and tubing, appliance gaskets/profiles, and synthetic leather.

Omnova Solutions acquired this product line with the Eliokem acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Particle Size 600 µmMedian
Mooney Viscosity 57
@Temperature 100 °C
ML 1+4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omnova Solutions Chemigum® P89 Nitrile Elastomer
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Omnova Solutions Chemigum® P86F Nitrile Elastomer
NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin
Omnova Solutions Chemigum® P7D Nitrile Elastomer

PELIO000 / 35682

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.