MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 4000 GF30 black Glass Fiber Reinforced PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: VESTAKEEP® 4000 GF30 black is a glass fiber reinforced (30%) polyether ether ketone for injection molding. The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 GF30 black are self-extinguishing. VESTAKEEP® 4000 GF30 black can be processed on common injection molding machines for thermoplastics. VESTAKEEP® 4000 GF30 black is supplied as cylindrical pellets in 25kg boxes with moisture-proof polyethylene liners. Pigmentation may affect the values.

Property data for dry samples.

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Moisture Absorption 0.0400 %ISO 15512
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4, 2577
Melt Flow 32 g/10 min
@Load 21.6 kg,
Temperature 400 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 11000 MPaISO 527
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
 75.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 175 Vtest solution A, 100 drops value; IEC 60112
 200 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 340 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 335 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 312 °CISO 75-1/-2
Vicat Softening Point 335 °CMethod B: 10 N, 50 K/h; ISO 306
 340 °CMethod A: 10 N, 50 K/h; ISO 306
Flammability Test 5.0
@Thickness 1.60 mm
IEC 60695-11-10
 5.0
@Thickness 3.20 mm
IEC 60695-11-10
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 400 °C
Mold Temperature 180 °C
 160 - 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK812 / 243021

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.