MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape
Categories: Polymer; Tape; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: 1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The following tests are conducted on one roll from each lot of tape per Mil-I-46852C: Thickness, Width, Bond Strength, Tensile Strength, Elongation, Dielectric Strength, and Water Absorption.

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccSilicone Property; Arlon SQA-TMS-024
Water Absorption 2.8 %2.8 %MIL-I-46852C
Thickness 508 microns20.0 milArlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Silicone Property; ASTM D2240
Tensile Strength, Ultimate 7.93 MPa1150 psiSilicone Property; ASTM D412
Elongation at Break 430 %430 %Silicone Property; ASTM D412
Adhesive Bond Strength 0.0214 MPa3.10 psiMIL-I-46852C
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 29.5 kV/mm750 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Wacker Elastosil® LR 3141/50 A/B Liquid Silicone Rubber
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer
Aremco Pyro-Tape™ 682-DS High Temperature Tape Double sided, single layer, fiberglass tape with silicone adhesive

PARL005 / 79657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.