MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo CALIBRE™ 200-3 Polycarbonate Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resistance, heat distortion resistance and optical clarity as well as high melt strength for sheet extrusion applications. Available in natural color only

Main Characteristics:

  • US FDA 21 CFR 177.1580
  • CSA
  • NSF
  • Underwriters Laboratory (UL)
  • EU food contact 200/72/EC
Applications:
  • Small appliances
  • Sheet and profile extrusion
  • Housewares

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/B; ASTM D792
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
0.15 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62; ASTM D570
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
0.32 %
@Temperature 73.4 °F
50% RH; ISO 62; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4; ASTM D955
Melt Flow 3.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
3.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7474ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength at Break 72.0 MPa10400 psiISO 527-2/50
 72.4 MPa10500 psi50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527-2/50; ASTM D638
Elongation at Break 150 %150 %50 mm/min; ISO 527-2/50; ASTM D638
Tensile Modulus 2.48 GPa360 ksi50 mm/min; ISO 527-2/50; ASTM D638
Flexural Strength 96.0 MPa13900 psi3-point; ISO 178
 96.5 MPa14000 psiMethod I (3 point load), 2.0 mm/min; ASTM D790
Flexural Modulus 2.41 GPa350 ksiMethod I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Izod Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO) 93.0 kJ/m²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256; ISO 180
Tensile Impact Strength 630 kJ/m²300 ft-lb/in²ASTM D1822
Dart Drop, Total Energy 93.8 J69.2 ft-lb3.39 m/sec; ASTM D3763
Abrasion 4545[%] Taber; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 60 Hz
3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
 17.0 kV/mm432 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 50 Hz
0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FUnannealed; ASTM D648; ISO 75-2/A
 143 °C289 °FAnnealed; ASTM D648; ISO 75-2/A
Vicat Softening Point 151 °C
@Load 5.10 kg
304 °F
@Load 11.2 lb
Rate A (50°C/h); ISO 306/B50; ASTM D1525
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Oxygen Index 26 %26 %ISO 4289-2
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542; ISO 489
Haze 1.0 %1.0 %ASTM D1003
Transmission, Visible 89 %89 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Average Extent of Burring3 cmASTM D635

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 200-6 Polycarbonate Resin
Trinseo CALIBRE™ 2061 HD 15 Polycarbonate Resin
Covestro Makrolon® 3103 Polycarbonate
Celanese Vandar® 8000 PBT, Unfilled
Celanese Vandar® 2500 PBT, Unfilled

PZZDWST030 / 142239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.