MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Trovicel® (19/24 mm) PVC Foam
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Product characteristics:
  • Low weight
  • Very high stiffness
  • Light and weather resistance
Product applications:
  • Visual communications
  • Construction industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.550 g/cc0.0199 lb/in³DIN EN ISO 1183-1
Water Absorption <= 0.20 %<= 0.20 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080DIN EN ISO 868
Modulus of Elasticity 0.700 GPa102 ksiDIN EN ISO 527
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 80.0 µm/m-°C33.3 - 44.4 µin/in-°FDIN 53752
Thermal Conductivity 0.0700 W/m-K0.486 BTU-in/hr-ft²-°FDIN 52612-1
Maximum Service Temperature, Air 60.0 °C140 °Flong term
Vicat Softening Point 75.0 °C167 °FDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air 0.000 °C32.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROCH9351 / 233053

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.