MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal solution for mono and coex film design.

Borsoft SD200CF is especially suitable for stationery folders, food/textile packaging, technical films, property modification in other applications fields, substitution of other plastics, and hygienic films

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 - 0.910 g/ccISO 1183
Thickness 50.0 microns
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 650 %ISO 527-3
Film Elongation at Break, TD 850 %ISO 527-3
Flexural Modulus 0.450 GPaISO 178
Secant Modulus, MD 0.200 GPaISO 527-3
Secant Modulus, TD 0.300 GPaISO 527-3
Impact 57.5Dynatest, Damaging Force (N); ISO 7765-2
Impact Test 1.60 JDynatest, Penetration Energy; ISO 7765-2
Film Tensile Strength at Break, MD 30.0 - 50.0 MPaISO 527-3
Film Tensile Strength at Break, TD 25.0 - 45.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 144 °CISO 3146
Vicat Softening Point 115 °CA (10N); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %ASTM D1003
 <= 8.0 %ASTM D1003
Gloss >= 20 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Total PPH 3860X Polypropylene, Extrusion Grade
Borealis SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Flint Hills 44S2A Polypropylene Impact Copolymer
Borealis BC142MO Polypropylene Copolymer

PBOREA104 / 27411

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.