MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Processed by selective laser sintering (SLS). Windform® RL is a durable thermoplastic elastomer material with exceptional rubber-like distinguishing features. Its mechanical characteristics make it particularly suited for Additive Manufacturing applications requiring complex geometries, and where flexible characteristics is a key requisite. It shows excellent durability and stability: it accommodates chemicals and heat resistance and combines superior tear resistance with burst strength. Windform® RL withstands repeated bending and deformation. It allows to manufacture accurate, reliable, and long lasting prototypes and durable end-use parts. It also guarantees accurate and superior surface finish and fine details. Windform® RL Shore A hardness value may vary in the range from 45 (Minimum) to 80 (Maximum). Due to its main properties, Windform® RL assures high performance sealing power. Windform® RL Seal Infiltration is a method for strengthening, coloring and sealing Windform® RL parts. Windform® RL Seal Infiltration enhances the strength at break and creates watertight barrier. It is available in a wide range of colors.

Application Examples: Functional rubber-like prototypes and parts (e.g. gaskets and hoses), durable components. Windform® RL is the material of choice for athletic footwear and equipment, and for all those parts requiring flexibility and good shock absorption. Its use allows to manufacture “soft-touch” items with non-slip surfaces e.g. handles and overmolded grips. Windform® RL is the material for simulating cast urethane, thermoplastic elastomer, rubber and silicone parts along with complex production, functional and F3 prototypes (prototypes to test form, fit and function). It is also suitable for parts that require joining with adhesives.

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 g/cc
Particle Size 160 µm100% Below 160 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45 - 80ASTM D2240
Tensile Strength at Break 1.50 - 4.20 MPaUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 130 - 160 %UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 0.00650 - 0.00800 GPaUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
 
Thermal PropertiesOriginal ValueComments
Melting Point 190.0 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
3D Systems DuraForm® PA Nylon for SLS® Systems
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
3D Systems DuraForm® Flex Thermoplastic Elastomer for SLS® Systems

PCRPT44m / 209868

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.