MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin resistance. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM262 is exceptionally good where high durometer and dimensional stability are required.

Key Features:

  • High Durometer
  • Low Viscosity
  • Casting resin resistance
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for architectural replication
  • Molds for polyester, epoxy resin casting
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccUncatalyzed, QM 262B
 1.26 g/ccBase
Viscosity 2000 cPUncatalyzed, QM 262B
 35000 cPcatalyzed with QM 262B
 45000 cPBase
Linear Mold Shrinkage 0.0010 cm/cmcured 72 hrs @ RT
Storage Temperature <= 38.0 °C12 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60cured 72 hrs @ RT
Tensile Strength 6.89 MPacured 72 hrs @ RT
Elongation at Break 150 %cured 72 hrs @ RT
Tear Strength 90.0 plicured 72 hrs @ RT
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 8 - 12 hourDemold time, catalyzed with QM 262B
Pot Life 60.0 mincatalyzed with QM 262B
 
Descriptive Properties
ColorBeigeBase
 Bluecatalyzed with QM 262B
 Light BlueUncatalyzed, QM 262B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fujipoly Industries Sarcon® 45H Thin-Film HR
CHT Group QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
CHT Group QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material
CHT Group QM 130T 30 Shore A, Translucent, Condensation Cure Moldmaking Material
CHT Group QGel 326 General Purpose Silicone Gel

PACC068 / 22195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.